Fiber Reinforced Concrete Beams Subjected to Combined Bending and Torsion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fiber Reinforced Concrete Beams Subjected to Combined Bending and Torsion

Author(s): Gordon Batson, Terry Terry, and Ming-Sung Chang

Publication: Symposium Paper

Volume: 81

Issue:

Appears on pages(s): 51-68

Keywords: beams (supports); bending; fiber reinforced concretes;loads (forces); metal fibers; torsion.

DOI: 10.14359/6445

Date: 11/1/1984

Abstract:
Test data using steel fibers as torsional shear reinforcement for 36 reinforced concrete beams subjected to combined bending and torsion are presented. Beams were loaded in bending at third points and by third point torsional loading. Straight steel fibers were 1.0 in (25.4 mm) long by 0.010 x 0.022 in (2.5 x 5.0 mm) in cross section and the volume percentages of fibers were 0.0, 0.5 and 1.0 and 1.5 percent. Test data were compared to a theory developed by Martin for concrete beams subjected to bending and torsion reinforced with longitudinal steel only, no closed stirrups. One volume percent or greater of straight steel fibers in combination with longitudinal torsional reinforcement were effective as torsional reinforcement for M/T ratios less than two. For M/T ratios greater than 10, 0.5 volume per cent was sufficient for torsional rein-forcement.