Flexural Fatigue Strength of Hybrid layered Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Fatigue Strength of Hybrid layered Concrete

Author(s): D. Y. lee, C. R. V. W. Heyveld, and F. W. Kloiber

Publication: Symposium Paper

Volume: 75

Issue:

Appears on pages(s): 253-268

Keywords: admixtures; beams (supports); bridge decks; concrete pavements; density (mass/volume); fatigue (materials); fatigue tests; flexural strength; latex (plastic); resurfacing; slump tests.

DOI: 10.14359/6410

Date: 9/1/1982

Abstract:
The results show that (a) the flexural fatigue life of normal concrete beams is higher than the fatigue life of layered beams utilizing dense concrete or latex modified concrete at lower stress levels but is lower than that of hybrid layered beams at higher stress levels and (b) essentially the same fatigue strength was obtained for beams containing only a 2-inch layer of either dense concrete or latex modified concrete at the surface as for beams containing these concretes full depth.