Refractory Problems and Repair Techniques in Refining and Petrochemical Operations

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Refractory Problems and Repair Techniques in Refining and Petrochemical Operations

Author(s): M.S. Crowley

Publication: Symposium Paper

Volume: 74

Issue:

Appears on pages(s): 117-124

Keywords: chemical attack; erosion; fiber reinforced concretes; furnaces; high temperature; incinerators; linings; petrochemistry; plants; refineries; refractory concretes; repairs; spalling.

DOI: 10.14359/6397

Date: 8/1/1982

Abstract:
Refining and petrochemical operations, such as fluid catalytic cracking units, naphtha reformers, incinerators, and furnaces subject refractory linings to a variety of aggressive actions, such as erosion, spalling, slagging, and chemical attack. A number of different types of monolithic refractory material are used to resist these actions. The types of refractory failure commonly experienced in refineries and petrochemical plants are discussed and methods of repairing or replacing the deteriorated areas are outlined. The effect of placement techniques, curing conditions, and start up procedures on the serviceability of repaired sections is also discussed.




  