Polymer Concrete for Electrical Applications

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Polymer Concrete for Electrical Applications

Author(s): Rosalia Torres Becerra

Publication: Symposium Paper

Volume: 69

Issue:

Appears on pages(s): 145-154

Keywords: aggregates; composite materials; economics; electrical insulators; manufacturing; methyl methacrylate; polyester resins; c o n c r e t e . Polymer

DOI: 10.14359/6384

Date: 8/1/1981

Abstract:
Polymer concrete has been successfully developed for use as an electrical insulating material. Work done at the Instituto de Investigaciones Electricas in Mexico has resulted in formulations using native materials and manufacturing techniques which promise to replace electrical porcelain in many instances. The technology and materials are especially suited to Mexico's requirements for electrical system expansion.