Performance History of Latex-Modified Concrete Overlays

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Performance History of Latex-Modified Concrete Overlays

Author(s): L. A. Kuhlmann

Publication: Symposium Paper

Volume: 69

Issue:

Appears on pages(s): 123-144

Keywords: bonding; bridge decks; bridges construction; corrosion; cracking (fractur field tests; history; latex (plastic); per Crete; repairs; resurfacing; reviews; skid (structures); concrete ing); deterioration; formance; polymer con-resistance.

DOI: 10.14359/6383

Date: 8/1/1981

Abstract:
Latex modified overlays have been in service for over 20 years. This report summarizes the significant events during the development of this system and highlights data that have recently been generated by State Highway Departments and the FHWA in their continuing studies of field performance. Fifteen reports, covering 184 bridge decks, aged two months to 13 years, are reviewed. Specific comments regarding test methods, such as chloride pen-etration and half-cell potential, to measure performance, are included. Life expectancy, based on the testing done to date, as well as the actual life in the field, is projected to be a minimum of 15-20 years.