Research in Progress: Rapid All-Weather Pavement Repair with Polymer Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Research in Progress: Rapid All-Weather Pavement Repair with Polymer Concrete

Author(s): Michael T. McNerney

Publication: Symposium Paper

Volume: 69

Issue:

Appears on pages(s): 93-106

Keywords: bombing; compressive strength; concrete durability; concrete pavements; curing; damage; explosions; high temperature; low temperature; metal fibers; methyl methacrylate; moisture;Michael T. McNerney

DOI: 10.14359/6381

Date: 8/1/1981

Abstract:
The Air Force Engineering and Services Center (AFESC) at Tyndall AFB, Florida is currently engaged in a seven-year research and development effort to rapidly repair bomb damaged concrete runways. Polymer concrete because of rapid cure and high strength is one of the most promising methods of repair. The problems of moisture, temperature extremes and mechanization are all being studied for development of a rapid all-weather polymer concrete repair system. Research includes work at the University of Texas at Austin, AFESC, Battelle Columbus Labora-tories, Brookhaven National Laboratory, and the BDM Corporation. Polymers being considered include acrylics, epoxies, polyesters and furans.