Survey and Rehabilitation of Parking Garage Decks-a Case Study

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Survey and Rehabilitation of Parking Garage Decks-a Case Study

Author(s): H. Ainso and T. M. Tronzo

Publication: Symposium Paper

Volume: 93

Issue:

Appears on pages(s): 671-694

Keywords: concrete slabs; construction joints; cracking (fracturing); deterioration; electric raceways; garages; parking facilities; repairs; waterproofing

DOI: 10.14359/6323

Date: 9/1/1986

Abstract:
Concrete parking decks are subject to several unique problems which can initiate or aggravate deterioration. These include negative-moment cracking, cold joint cracking, cracking due to embedded conduit runs, and other water related damage. This paper will deal with these problems encountered during the rehabilitation of the parking decks in a 3-story, 28-year-old garage. This structure was not maintained for its entire life, except for the installation of a waterproofing membrane on the top deck about 8 years ago. The topics covered are: 1) inspection and testing what to look for and specific test procedures; 2) causes and recommendations for the repair of some of the problems encountered.