Workability, Testing, and Performance of Self-Consolidating Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Workability, Testing, and Performance of Self-Consolidating Concrete

Author(s): K. H. Khayat

Publication: Materials Journal

Volume: 96

Issue: 3

Appears on pages(s): 346-353

Keywords: bleeding (concrete); consolidation; high-performance concrete; rheological properties; segregation; stability; viscosity; workability

DOI: 10.14359/632

Date: 5/1/1999

Abstract:
Self-consolidating concrete is a new category of high-performance concrete that exhibits a low resistance to flow to insure high fallibility and a moderate viscosity to maintain a homogeneous deformation through restricted sections, such as closely-spaced reinforcement. Self-consolidating concrete is used to improve the productivity of casting congested sections and insure the proper filling of restricted areas with minimum or no consolidation. Such concrete can improve the homogeneity of highly fellable concrete that is necessary to insure good bond development with reinforcing steel, adequate structural performance, and proper durability. This paper reviews the benefits of using self-consolidating concrete to facilitate the casting of densely reinforced sections and improve productivity and on-site working conditions. Workability requirements necessary to secure self-consolidation and the principles involved in proportioning such highly fellable concrete are discussed. Field-oriented tests are useful to evaluate the deformability, filling capacity, and stability of self-consolidating concrete are presented. The performance of concrete mixes proportioned according to two main approaches needed to insure high deformability, low risk of blockage during flow, and proper stability are compared. Such approaches involved the proportioning of concrete with moderate water-to-cementitious material ratios of 0.35 to 0.38 to reduce free water content and provide stability. Mixes with both moderate and high contents of ternary cementitious materials were evaluated. The performance of each concrete was compared to that of a flowable concrete with 250-mm slump.