Heat Curing and Late Formation of Ettringite

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Heat Curing and Late Formation of Ettringite

Author(s): V. Johansen and N. Thaulow

Publication: Symposium Paper

Volume: 177

Issue:

Appears on pages(s): 47-64

Keywords: curing; ettringite; expansion; models; sulfate attack

DOI: 10.14359/6227

Date: 1/1/1999

Abstract:
Paste, mortar, and concrete cured at temperatures above certain limits may exhibit expansion and cracking during subsequent exposure to varying moist conditions. This phenomenon originally became known as delayed ettringite formation, DEF. DEF results in a typical microstructure which is demonstrated with examples from field samples and laboratory-made samples. The microstructure is compared with examples of internal sulfate attack in laboratory samples. These typical features include gaps around the aggregate where the paste shows an almost perfect replica of the individual aggregate surfaces. Expansion of the paste on a scale which is homogeneous relative to the aggregate would lead to such features. The chemistry in DEF is similar to that of sulfate attack. A mechanism involving hydrates of aluminates and possible unhydrated cement clinker particles is discussed.