Improved Superplasticized Precast Concrete Tiles

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Improved Superplasticized Precast Concrete Tiles

Author(s): G. Ferrari, V. Riunno, D. Salvioni and P. Tassone

Publication: Symposium Paper

Volume: 173

Issue:

Appears on pages(s): 953-972

Keywords: Acrylic resins; electron microscopes; precast concrete; stability; superplasticizers; tiles

DOI: 10.14359/6221

Date: 9/1/1997

Abstract:
Concrete tiles were produced according to a new technology based on a vacuum treatment combined with a vibro-compacting placement of superplasticized mixture. Three concrete mixtures (all vibro-compacted according to this technique) were manufactured with different water-cement ratio (0.50 or 0.32) and in the absence or in the presence of the vacuum treatment. Measurements of flexural strength, dimensional stability, SEM, image analysis and particle size distribution of anhydrous cement in concrete tiles were carried out. The vacuum treatment, which removed entrapped air voids from the fresh mixture during the vibro-compacting placement, increased flexural strength but did not change the dimensional stability. The reduction in the W/C from 0.50 to 0.32 significantly increased flexural strength. It also improved the dimensional stability in terms of a lower curling effect caused by different humidity exposures of the two opposite faces of the .concrete tile. The combination of vacuum treatment with low W/C produces a macro-defect free and low micro-porosity cement matrix which is responsible for the high strength and low curling effect of these concrete tiles.