Superplasticized Microcement Grouts

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Superplasticized Microcement Grouts

Author(s): M. C. Santagata, G. Bonora and M. Collepardi

Publication: Symposium Paper

Volume: 173

Issue:

Appears on pages(s): 909-936

Keywords: Grouting; microconcretes; rheological properties; soils; superplasticizers

DOI: 10.14359/6219

Date: 9/1/1997

Abstract:
The paper examines the rheological and mechanical behavior of super-plasticized microcement grouts to be used for the consolidation of porous systems (e.g. sand deposits, masonry walls of historical buildings). Five microcements were used: they differed in chemical composition of the clinker, type of mineral addition (natural pozzolan or silica fume), and particle size distribution. Three different super-plasticizing chemical admixtures - acrylic, naphtalene, and melamine based - were used, all with an active polymer content of 0.4% by mass of cement. The following properties of the grouts were investigated compressive strength, stability (bleeding test). fluidity (Marsh cone), The acrylic polymer proved to be more effective than the naphtalene and melamine based products in reducing the mixing water to produce a given initial fluidity. Furthermore, the grouts produced with this super-plasticizer displayed a lower fluidity loss with time. The performance of a specific mixture was also strongly dependent on the fineness of the binder and on the type of mineral addition. The compressive strength of the hardened grouts was primarily affected -especially at latter ages - by the water-binder ratio, independently of the type of super-plasticizer. None of the mixtures considered showed any significant bleeding. A limited number of injection tests in columns of dense sand were also performed. For a given water binder ratio, the groutability of a mixture was greatly improved using the acrylic based super-plasticizer in place of the melamine- and naphtalene-based products.