Title: Effective Use of Lithium-Based Admixtures for Set Control of Cementitious Systems

Author(s): H. Wang, K. Eubanks, B. Fitch, C. Manissero and F. Marin

Publication: Symposium Paper

Volume: 173

Issue:

Appears on pages(s): 893-908

Keywords: accelerating agents; admixtures; blending; calcium aluminate hydrates; lithium; portland cement; setting (hardening)

DOI: 10.14359/6218

Date: 9/1/1997

Abstract:
This paper describes the development and applications of several lithium-based chemical admixtures for set control of cementitious-based construction and building materials. Comparative evaluations show the effect of these admixtures on the set time of (1) calcium aluminate cement; (2) portland cement; and (3) blended systems of calcium aluminate cement and portland cement. General information is provided to address the principles of material selection, dosage rate and application of cementitious systems.