Study on the Ability of Highly-Flowable Concrete to Pass Between Steel Reinforcing Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on the Ability of Highly-Flowable Concrete to Pass Between Steel Reinforcing Bars

Author(s): Hiromi Fujiwara, Shigeyoshi Nagataki, Akito Dozono and Akira Obatake

Publication: Symposium Paper

Volume: 172

Issue:

Appears on pages(s): 397-412

Keywords: Coarse aggregates; reinforced concrete; reinforcing steels; tests

DOI: 10.14359/6143

Date: 12/1/1999

Abstract:
Highly flowable concrete has been receiving particular attention in recent years. With highly flowable concrete, the use of a vibrator for consolidating is not necessary because the concrete is self-consolidating within the form. To produce self-consolidating highly flowable concrete, the concrete must have high fluidity, resistance to segregation and the ability to pass between steel reinforcing bars. For this paper, one of these properties, the ability to pass between steel reinforcing bars was studied. The mechanism of coarse aggregate accumulation between the bars, considered the main factor influencing this ability, was studied and then confirmed through execution of two experiments. Based on the results of these experiments, the conditions related to volume and shape of coarse aggregate contained in the concrete and the clearance between and direction of the steel reinforcing bars which would permit the coarse aggregate to pass between the bars were clarified.