Title: Durability of a Notable Concrete Project

Author(s): James Warner and Edward K. Rice

Publication: Concrete International

Volume: 19

Issue: 8

Appears on pages(s): 53-55

Keywords: cantilever beams; durability; driveways;

DOI:

Date: 8/1/1997

Abstract:
A private residence was built on a steep ridge in California in the 1950s that used an innovative and creative concrete design. The spiral, cantilevered, prestressed driveway provides access to the "house on the hill" and 40 years later, it still exhibits durability.