HPC Precast Sewer Pipe

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: HPC Precast Sewer Pipe

Author(s): D.O. Northwood, Kevin Cail and Kevin A. MacDonald

Publication: Symposium Paper

Volume: 171

Issue:

Appears on pages(s): 201-208

Keywords: Chlorides; diffusivity; durability; precast concrete; silica fume.

DOI: 10.14359/6097

Date: 8/1/1997

Abstract:
Recently, a major North American City replaced a large collector sewer which was deteriorated due to corrosion of the reinforcement. This replacement was well in advance of the life cycle estimate of the pipe. The deterioration was caused predominately by the presence of chloride ion in the soils. As a part of this reconstruction, it was decided to design the concrete to resist the intrusion of chloride ion. Several proprietary admixtures were considered, as well as the use of silica fume, to produce this pipe. The contract was awarded to a conventional dry process pipe plant. Some modification of the mixture proportions was required. An interground silica fume cement was used to reduce the handling difficulties associated with silica fume. A preconstruction trial batch was evaluated for physical properties, including rapid chloride permeability and chloride ion diffusivity. The cost effectiveness of the modified cement and the relatively simple adjustments to the casting process resulted in a very minimal increase in the total construction cost. Design calculations and quality control methods are discussed.