Title: Seismic Retrofitting of Bridge Foundations

Author(s): David I. McLean and M. Lee Marsh

Publication: Structural Journal

Volume: 96

Issue: 2

Appears on pages(s): 174-182

Keywords: bridges (structures) columns (supports); ductility; earthquake resistant structures; foundations; shear strength

DOI: 10.14359/608

Date: 3/1/1999

Abstract:
This paper describes an experimental study investigating retrofitting measures for improving the seismic performance of the foundations of existing bridges. Retrofit measures for both pile-supported and spread footings were investigated. Tests were conducted on 1/3-scale footing and column assemblages that incorporated details selected to represent deficiencies common in older bridges. Tests on the as-built specimens resulted in a brittle failure due to insufficient joint shear strength in the column- footing connection. An added reinforced concrete overlay provided an effective retrofit for the as-built footings. In specimens that were overturning critical, increased overturning resistance was achieved by enlarging the footing plan size, by providing additional piles, or by providing tie-downs through the footing.