Rapid Testing Methods for Segregation Resistance and Filling Ability of Self-Compacting Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rapid Testing Methods for Segregation Resistance and Filling Ability of Self-Compacting Concrete

Author(s): B.K. Van, D.G. Montgomery, I. Hinczak and K. Turner

Publication: Symposium Paper

Volume: 179

Issue:

Appears on pages(s): 85-104

Keywords: deformation; self-compacting concrete; tests

DOI: 10.14359/6033

Date: 6/1/1998

Abstract:
This paper describes rapid testing methods for determining blocking behaviour, deformability and segregation resistance of self-compacting concrete. Laboratory test results have shown that the proposed methods can reduce the required extent of laboratory testing and enable the tests to be carried out in less time. A simple apparatus for segregation resistance testing is also proposed. This apparatus and modified L-box apparatus are considered useful for rapid testing of segregation resistance, deformability and blocking behaviour of fresh self-compacting concrete.