Cracking Tendency of High Strength Lightweight Aggregate Concrete at Early Ages

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cracking Tendency of High Strength Lightweight Aggregate Concrete at Early Ages

Author(s): T .A . Hammer , O. Bjontegaard and E. J. Sellevold

Publication: Symposium Paper

Volume: 179

Issue:

Appears on pages(s): 53-64

Keywords: aggregates; cracking (fracturing) high-strength concrete; strains; stresses

DOI: 10.14359/6031

Date: 6/1/1998

Abstract:
The use of high strength normal weight and lightweight aggregate concrete (i.e. with water/binder ratios below 0.40) have shown that the concrete may be more sensitive to cracking the first hours and days after casting (due to autogenous shrinkage and thermal strains), than normal strength concretes. Two test rigs have been built in order to investigate the problem. The Shrinkage-Rig determines the free deformations (e.g. autogenous and thermal deformations), and the special Stress-Rig determines the stresses when the concrete is restrained against the deformations. The paper presents the results from testing of one high strength normal weight concrete and one high strength lightweight aggregate concrete, both with water/binder ratio 0.38, in the test rigs. Both concretes were exposed to two different temperature histories generated from heat of hydration. The normal weight concrete developed relatively high tensile strains during the cooling phase. The corresponding stresses in the Stress-Rig became very high, and in one case the concrete failed. The lightweight aggregate concrete, however, did not develop any tensile strain, due to a lack of autogenous shrinkage caused by the water supply from the LWA grains. Consequently, no severe tensile stresses were built up in the Stress-Rig.