Compressive Strength of Portland Blast Furnace Slag Cement Concrete in Adiabatic and Semi-Temperature Matched Curing Conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compressive Strength of Portland Blast Furnace Slag Cement Concrete in Adiabatic and Semi-Temperature Matched Curing Conditions

Author(s): J.L. Yang, E.Y. Chen, G.L. Low and B.T. Tan

Publication: Symposium Paper

Volume: 178

Issue:

Appears on pages(s): 857-874

Keywords: adiabatic temperature; chloride permeability; compressive strength; curing; temperature.

DOI: 10.14359/6012

Date: 6/1/1998

Abstract:
Various grades of portland blast furnace slag cement (PBFC) and normal portland cement (OPC) concrete have been cured under adiabatic and semi-temperature matched curing conditions. Comparisons of the compressive strength between adiabatic, semi-temperature matched and ambient cured concrete have been made. The results indicated that the curing history had significant influence on the compressive strength development and the in-situ early strength of PBFC concrete is comparable to the same grade of OPC concrete after three days. The high curing temperature (above 65°C) reduced the later-age strength both for PBFC and OPC concrete. The durability of the concrete cured under various conditions was also evaluated by rapid chloride permeability test.