Engineering Properties of Concretes with Combinations of Cementitious Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Engineering Properties of Concretes with Combinations of Cementitious Materials

Author(s): R.N. Swamy and A.A. Darwish

Publication: Symposium Paper

Volume: 178

Issue:

Appears on pages(s): 661-684

Keywords: fly ash; slag; silica fume; pozzolans; compressive strength; flexural strength; dynamic modulus.

DOI: 10.14359/6002

Date: 6/1/1998

Abstract:
The overall objective of this paper is to establish the engineering properties of concrete containing combinations of fly ash/silica fume and slag/silica fume. Six concrete mixtures were tested, with total cementitious materials content of 350 kg/m3 and 450 kg/m3, and a constant water/cementitious materials ratio of 0.45. The effect of three curing conditions was investigated, and the tests were performed up to about 260 days. The results reflect conclusively that cement replacement materials reduce slightly the engineering properties of portland cement concrete, and that the exposure conditions have a strong influence on flexural strength, dynamic modulus, and ultrasonic pulse velocity. Slag was generally found to be slightly superior to fly ash in the development of these engineering properties. The key to developing fly ash/silica fume and slag/silica fume concretes without suffering a reduction of strength gain when exposed to drying environmental conditions is to incorporate within the mixtures adequate amounts of portland cement and water to ensure the continuation of pozzolanic reactivity and hydration.