U.S.-Japan Cooperative Research Program on Composite and Hybrid Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: U.S.-Japan Cooperative Research Program on Composite and Hybrid Structures

Author(s): Subhash C. Goel

Publication: Symposium Paper

Volume: 174

Issue:

Appears on pages(s): 213-224

Keywords: Columns; composite construction; eathquakes; reinforced concrete; walls

DOI: 10.14359/5966

Date: 4/1/1998

Abstract:
A five-year research program on Composite and Hybrid Structures as Phase 5 of the U.S.-Japan cooperative Earthquake Research Program was recommended to be initiated in 1993 in both countries. Presented in this paper is a summary of the research program which is based on a number of technical meetings of the U.S. and Japan Planning Groups and a Joint Planning Workshop. Because of diverse and broad scope of the subject area, the research program is organized into the following four groups: New Materials, Elements and Systems; Concrete Filled Tube Column Systems; Reinforced Concrete (RC) and Steel Reinforced Concrete (SRC) Column Systems; and RC/SRC Wall Systems. A theme structure with well selected layout, geometry and design loads for the research is also presented, which provides a common focus for various systems to be studied, and also a common prototype structure from which the components and sub-assemblages are drawn.