Toward a Rational Approach for Design of Minimum Torsion Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Toward a Rational Approach for Design of Minimum Torsion Reinforcement

Author(s): Mohamed A. Ali and Richard N. White

Publication: Structural Journal

Volume: 96

Issue: 1

Appears on pages(s): 40-45

Keywords: beams; brittleness (brittle failure); minimum reinforcement; reinforced concrete; structural design; torsion

DOI: 10.14359/594

Date: 1/1/1999

Abstract:
One of the significant improvements in ACI 318-95 is the adoption of a rational model for torsion design. The minimum torsional reinforcement requirement remained empirical. This paper describes a proposed rational approach for computing minimum torsional reinforcement.