Premixed Epoxy Polymer Concrete Bridge Deck Overlays

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Premixed Epoxy Polymer Concrete Bridge Deck Overlays

Author(s): Floyd E. Dimmick, Sr.

Publication: Symposium Paper

Volume: 169

Issue:

Appears on pages(s): 146-171

Keywords: Bridge decks; epoxy resins; freeze-thaw durability; polymer concrete; portland concrete; resurfacing

DOI: 10.14359/5936

Date: 5/1/1997

Abstract:
bridge, decks, ramps and roadways utilizing portland cement B concrete [PCC] that need protection from natural environmental conditions such as wet/dry cycles, freeze-thaw, chlorides from soil [ 11, water or deicing salts, erosion, and abrasion f?omvehicular traffic can be protected with micro-thin epoxy polymer concrete overlays. This paper presents a brief review of three bridge deck overlays in the United States that comply with AASHTO-AGC-ARTBA Task Force 34, Chapter 4, Epoxy Polymer Concrete Overlays [2]. It provides information when to use Epoxy Polymer Concrete [EPC] Overlays, how to place the overlay, equipment options, surface profile selection, physical properties of the EPC and commentary on each project.