5-Year Performance of Overlays in Fort Worth, Texas

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 5-Year Performance of Overlays in Fort Worth, Texas

Author(s): Jamal-Aldin H. Zalatimo and David W. Fowler

Publication: Symposium Paper

Volume: 169

Issue:

Appears on pages(s): 122-145

Keywords: Bridge decks; cracking (fracturing); epoxy resins; methyl methacrylate; polyester resins; polymer concrete; resurfacing

DOI: 10.14359/5935

Date: 5/1/1997

Abstract:
Several overlay test sections were placed on two bridge decks and a section of a concrete approach pavement in Fort Worth, Texas, about five years ago. Different monomers, primers, mix designs, and construction methods were used. The same materials were investigated extensively in the laboratory. The test sections were open to regular traffic and tested several times over the past five years. The results and conclusions of this experimental program are presented here.