Behavior of High-Strength High-Performance Concrete Bridge Girders

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of High-Strength High-Performance Concrete Bridge Girders

Author(s): J. F. Stanton, P. Barr, and M. O. Eberhard

Publication: Symposium Paper

Volume: 189

Issue:

Appears on pages(s): 71-92

Keywords: bridge girders; camber; high-performance concrete; high-strength concrete; instrumentation; prestress; strains; thermal effects

DOI: 10.14359/5846

Date: 1/1/2000

Abstract:
This paper describes the measured behavior of a bridge made with precast, prestressed, high-performance concrete (HPC) girders. The concrete was considered high-performance, because it was specified to have a compressive strength of 51 MPa (7400 psi) at release and 69 MPa (10,000 psi) at 56 days. By using HPC instead of normal-strength concrete, the bridge designer was able to reduce the number of girder lines from seven to five. These girders were the first to be constructed in Washington State using HPC. To monitor the girders, vibrating-wire strain gages with thermistors were installed in five girders, and camber was monitored by various means, including a stretched-wire system that could be monitored by the data-aquisition system. Temperatures measured during fabrication indicate the presence of a large and unexpected temperature gradient over the height of the girder. As a result the concrete strength at release may have been lower at the bottom of the girder than at the top. The long-span girders were stressed to an initial bottom stress of approximately 28 MPa (4000 psi). The strength of the concrete was higher than usual and permitted the high initial stress. However elastic modulus rises only with the square root of strength, so elastic shortening strains, and creep strains that are assumed to depend on them, are higher for high-strength concrete. In these girders, elastic shortening and creep dominated the loses. The measured losses were compared with the predicted losses form two standard methods, but neither method was able to provide a universally superior match. In general, the measured losses exceeded the calculated losses initially, but with time, the discrepancies decreased.