Slurries for Restoration of Historical Brickwork Buildings in Northern Germany

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Slurries for Restoration of Historical Brickwork Buildings in Northern Germany

Author(s): K. G. Bottger and D. Knofel

Publication: Symposium Paper

Volume: 193

Issue:

Appears on pages(s): 37-62

Keywords: blast-furnace slag; cement; hydraulic hydrated lime;

DOI: 10.14359/5812

Date: 8/1/2000

Abstract:
This contribution deals with the development of slurries for the restoration of brickwork buildings in Northern Germany. Various slurries on the basis of two binders with a high sulphate resistance with an admixture of solid glass globules respectively were developed, one slurry on the basis of lime the other on the basis of cement. Their aggregate is of fine quartz sands and various additives were used. The slurries were developed to restore historical terracotta. Beside the workability and the water retention capacity of the slurries, technological pa-rameters such as dynamic modulus of elasticity, compressive strength, bending and bond strength and hygrical parameters such as water absorption, water desorptions and water vapour diffusion were investigated. Further important characteristics were the resistance to freezing and thawing, the scuff resistance and the efflorescence behaviour. Some of the slurries were successfully applied to the terracotta surfaces.