Influence of Polymer Modification on Durability of Porous Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Polymer Modification on Durability of Porous Concrete

Author(s): A. Beeldens, D. Van Gemert, C. Caestecker, M. Van Messem, and E. De Winne

Publication: Symposium Paper

Volume: 192

Issue:

Appears on pages(s): 773-788

Keywords: deicing; freeze-thaw durability; polymerization; porosity; thermal gradient; wetting and drying tests

DOI: 10.14359/5784

Date: 4/1/2000

Abstract:
Porous concrete is used as top layer on highway roads and is characterized by a very open structure due to the use of gap-graded aggregates. This provides good drainage capabilities and noise reducing properties. In a preliminary test program, the durability of concrete, a polymer emulsion was added to the concrete mixture. Three different types of polymer emulsions were used. The resistance against freezing and thawing cycles, deicing salts, temperature variation and wetting and drying cycles were investigated on samples with a polymer-cement ratio of .10. Minimum film forming temp4erature, strength and elasticity of the polymer emulsion and of the hardened polymer film were determine as well. This paper deals with the results of the durability tests and investigates the relation between the properties of the polymer emulsion and the behavior of the polymer modified porous concrete. The role of the polymer film concerning structure formation as well as durability behavior in the hardened concrete is discussed.