Reinforcing Effects of Processed Cellulose Fibers in Mortar (Stucco), Thin Sheet products, and Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reinforcing Effects of Processed Cellulose Fibers in Mortar (Stucco), Thin Sheet products, and Concrete

Author(s): P. Soroushian

Publication: Symposium Paper

Volume: 190

Issue:

Appears on pages(s): 203-212

Keywords: aggregates; cellulose fibers; durability

DOI: 10.14359/5729

Date: 4/1/2000

Abstract:
This paper reviews the key effects of processed cellulous fibers at practi-cal dosage rates in cement-based mixtures of different cement contents and aggregate particle sizes, produced by normal casting or using different thin sheet processing systems. Mechanical characteristics, restrained plastic and drying shrinkage cracking attributes, and durability characteristics under dif-ferent accelerated aging conditions are investigated. Performance character-istics of processed cellulose fibers in thin sheet cement products subjected to . different processing systems are compared.