Nonlaminated Pin-Loaded Carbon Fiber Reinforced Plastic Straps for Shear Enhancement of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Nonlaminated Pin-Loaded Carbon Fiber Reinforced Plastic Straps for Shear Enhancement of Concrete

Author(s): J. M. Lees, A. Winistoerfer, and U. Meier

Publication: Symposium Paper

Volume: 188

Issue:

Appears on pages(s): 985-994

Keywords: carbon fiber reinforced plastics; concretes; repair; shear; strengthening

DOI: 10.14359/5686

Date: 8/1/1999

Abstract:
Increasingly, existing concrete structures are being assessed as having insufficient capacity in shear; the development of an efficient and durable means of upgrading such structures is becoming of utmost importance. An exciting solution is the use of tensioned non-laminated carbon fiber reinforced plastic (CFRP) straps as active (stressed) external shear reinforcement for concrete. The use of an active system has several advantages over a passive (unstressed) reinforcement system. In particular, the prestressed CFRP straps provide confinement and enhance the performance of the concrete. Details of a series of tests carried out on a concrete beam strengthened using these novel CFRP shear reinforcing elements are presented. The strain in each of the straps was measured during testing and valuable insight into the shear behaviour of the concrete beam was gained. It was found that the strengthened beam had a much higher shear capacity than the predicted resistance of an equivalent unstrengthened beam.