Concrete Cover Delamination in Reinforced Concrete Beams Strengthened with Carbon Fiber Reinforced Polymer Sheets

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Cover Delamination in Reinforced Concrete Beams Strengthened with Carbon Fiber Reinforced Polymer Sheets

Author(s): G. Tumialan, P. Serra, A. Nanni, and A. Belarbi

Publication: Symposium Paper

Volume: 188

Issue:

Appears on pages(s): 725-736

Keywords: carbon fiber reinforced polymer sheets; ductility; flexural

DOI: 10.14359/5667

Date: 8/1/1999

Abstract:
In addition to the conventional modes of failure observed in RC beams, new ones can be detected in RC members strengthened by means of externally bonded FRP reinforcement. Concrete cover delamination is a mode of failure caused by shear transfer and local regions of tension stress fields. A series of tests were carried out in order to study the concrete cover delamination failure, wherein the variables were length of beam span, bonded area, number of plies, and U-jacketing schemes. Two mechanisms within the concrete cover delamination failure were observed: one starting at the cutoff point of the FRP, which is originated by a high concentration of normal (out-of-plane) and shear stresses, and second one starting at an intermediate crack. The latter mode of failure is caused by normal and shear stresses at the level of the steel reinforcement. From the point of view of design, it is important to recognize this premature type of failure, and determine algorithms for its prediction.