Title: Twisting Moments in Two-Way Slabs

Author(s): Myoungsu Shin, Allan Bommer, James B. Deaton, and Bulent Alemdar

Publication: Concrete International

Volume: 31

Issue: 7

Appears on pages(s): 35-40

Keywords: design; finite element analysis; torsion; two-way slab

DOI:

Date: 7/1/2009

Abstract:
In contrast to traditional strip methods for two-way slab design, finite element analysis (FEA) automatically provides deformation compatibility and a full equilibrium load path. Designers using FEA, however, have often blindly ignored twisting moments that occur on the edges of the elements because they are not sure how to account for them. This assumption may be unconservative where torsion is high. The available methods for explicitly incorporating twisting moments in the design of slabs based on FEA results are discussed in this article.