Title: SP-260: Fabrication Technology for Thin Cementitious Products

Author(s): Editors: Yixin Shao and Ashish Dubey / Sponsored by: ACI Committee 549

Publication: Symposium Paper

Volume: 260

Issue:

Appears on pages(s): 180

Keywords:

DOI: 10.14359/56604

Date: 6/1/2009

Abstract:
This CD-ROM consists of papers that were presented at a session sponsored by Committee 549 at the Fall 2007 Convention in Fajardo, Puerto Rico. The objective of the symposium was to have a state-of-the-art review on the development of fabrication methods for cementitious products and explore their potential market opportunity in residential and industrial building applications. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-260