ACI Student Fellowships, Scholarships for 2009-2010

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI Student Fellowships, Scholarships for 2009-2010

Author(s):

Publication: Concrete International

Volume: 31

Issue: 6

Appears on pages(s): 26-28

Keywords:

DOI:

Date: 6/1/2009

Abstract:
For the 2009-2010 academic year, ACI has awarded eight Student Fellowships and five Graduate Scholarships.