Study on minimum shear reinforcement of flat slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on minimum shear reinforcement of flat slabs

Author(s): A. P. R. VAZ, R. B. GOMES, L. C. D. SHEHATA

Publication: IBRACON

Volume: 2

Issue: 1

Appears on pages(s): 01-24

Keywords: flat slabs, minimum shear reinforcement, reinforced concrete.

DOI:

Date: 3/30/2009

Abstract:
In a preliminary study that aims to define the minimum shear reinforcement of flat slabs that, leading to a punching shear failure surface that crosses that reinforcement, can avoid a sudden failure, nine slabs with 1800 mm x 1800 mm x 130 mm dimensions were tested. Their main variables were the number of shear reinforcement layers of the stud type, the cross-section area of that reinforcement in each circumferential layer and the diameter of the studs. In the attempt to define the minimum punching reinforcement of the slabs, a parameter ?, equal to the total force in the transverse reinforcement inside a truncated cone bounded by the shear crack divided by the punching strength of a similar slab without shear reinforcement, was used. The values of ? of the slabs varied between 0.27 and 1.03 and the punching failure surface crossed the shear reinforcement when ? was smaller than around 0.70. The value of ? equal to 0.6 was defined as close to the minimum for slabs with effective depth of 90 mm and flexure reinforcement ratio of 1.38%. In comparison with the slab with no shear reinforcement, slabs having ? of that order had a punching strength and rotation increase of about 10% and 30%, respectively