Numerical Fracture analysis of prestressed concrete beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Numerical Fracture analysis of prestressed concrete beams

Author(s): Timon Rabczuk and Goangseup Zi

Publication: IJCSM

Volume: 2

Issue: 2

Appears on pages(s): 153-160

Keywords: reinforced concrete; meshfree methods; fracture; cohesive models

DOI:

Date: 12/31/2008

Abstract:
Fracture of prestressed concrete beams is studied with a novel and robust three-dimensional meshfree method. The meshfree method describes the crack as a set of cohesive crack segments and avoids the representation of the crack surface. It is ideally suited for a large number of cracks. The crack is modeled by splitting particles into two particles on opposite sides of the crack segment and the shape functions of neighboring particles are modified in a way the discontinuous displacement field is captured appropriately. A simple, robust and efficient way to determine, on which side adjacent particles of the corresponding crack segment lies, is proposed. We will show that the method does not show any ”mesh” orientation bias and captures complicated failure patterns of experimental data well.