Experimental Study on Bond-Slip Behavior of Longitudinal Bars in Reinforced Concrete Beams Confined with Fiber Reinforced Polymer Sheets

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study on Bond-Slip Behavior of Longitudinal Bars in Reinforced Concrete Beams Confined with Fiber Reinforced Polymer Sheets

Author(s): S. Kono, K. Matsuno, and T. Kaku

Publication: Symposium Paper

Volume: 188

Issue:

Appears on pages(s): 333-346

Keywords: bond strength; confinement; failure; fiber reinforced

DOI: 10.14359/5635

Date: 8/1/1999

Abstract:
Twenty cantilever type specimens and four beam specimens were tested to evaluate the bond behavior in reinforced concrete members confined with carbon or aramid FRP sheets. The main test variables were the vertical cover depth, the diameter and the number of longitudinal bars, and the type and the amount of FRP sheets. The test results showed that the confined specimens had higher bond strength, larger peak load slip displacement and lesser bond degradation after the peak than their unconfined prototype counterparts. Based on the test results, an equation was developed to predict the increase in bond strength due to the FRP sheet confinement. That increase was expressed similarly to that due to transverse steel reinforcement except that the elastic modulus of the FRP sheet was important but the number of longitudinal bars was not. The proposed equation was validated using results of column specimens tested in other research institutes and by cantilever and beam specimens tested by authors. It was proved that as long as the bond strength of an unconfined prototype specimen is evaluated properly, the total bond strength of confined specimens can be predicted accurately using the proposed equation although the limitations of the proposed equation still need to be clarified.