Numerical Simulation of Wave Propagation in Mortar with Inhomogeneities

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Numerical Simulation of Wave Propagation in Mortar with Inhomogeneities

Author(s): Dimitrios G. Aggelis and Shouhei Momoki

Publication: Materials Journal

Volume: 106

Issue: 1

Appears on pages(s): 59-63

Keywords: damage assessment; dispersion; nondestructive testing; pulse velocity; simulation

DOI: 10.14359/56317

Date: 1/1/2009

Abstract:
In this paper, wave propagation in concrete with inhomogeneity is examined using numerical simulations. Simulated damage is filmshaped to resemble the actual shape of cracks. Results of pulse velocity and wave distortion are compared with experimental ones, showing good agreement. It is concluded that, apart from the volume content, the characteristic shape and orientation of damage are crucial for wave propagation influencing the correlations between velocity and damage.