Flow and Compressive Strength of Alkali-Activated Mortars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flow and Compressive Strength of Alkali-Activated Mortars

Author(s): Keun-Hyeok Yang, Jin-Kyu Song, Kang-Seok Lee, and Ashraf F. Ashour

Publication: Materials Journal

Volume: 106

Issue: 1

Appears on pages(s): 50-58

Keywords: alkali-activated mortar; fly ash; slag; neural network; regression analysis

DOI: 10.14359/56316

Date: 1/1/2009

Abstract:
Test results of 36 slag-based mortars and 18 fly ash (FA)-based mortars activated by sodium silicate and/or sodium hydroxide powders are presented. The main variables investigated were the mixing ratio of sodium oxide (Na2O) of the activators to source materials, water-binder ratio (w/b), and fine aggregate-binder ratio (s/b). Test results showed that slag-based alkali-activated (AA) mortars exhibited much higher compressive strength but slightly less flow than FA-based AA mortars for the same mixing condition. Feed-forward neural networks and simplified equations developed from nonlinear multiple regression analysis were proposed to evaluate the initial flow and 28-day compressive strength of AA mortars. The training and testing of neural networks and the calibration of the simplified equations were achieved using a comprehensive database of 82 test results of mortars activated by sodium silicate and sodium hydroxide powders. Compressive strength development of slag-based AA mortars was also estimated using the formula specified in ACI 209R calibrated against the collected database. Predictions obtained from the trained neural network or developed simplified equations were in good agreement with test results, although early strength of slag-based AA mortars was slightly overestimated by the proposed simplified equations.


ALSO AVAILABLE IN:

Electronic Materials Journal