Seismic Rehabilitation of Unreinforced Masonry Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Rehabilitation of Unreinforced Masonry Walls

Author(s): O. S. Marshall, Jr., S. C. Sweeney, and J. C. Trovillion

Publication: Symposium Paper

Volume: 188

Issue:

Appears on pages(s): 287-296

Keywords: composites; fiber reinforced polymer; masonry;

DOI: 10.14359/5630

Date: 8/1/1999

Abstract:
The U.S. Army Construction Engineering Research Laboratory, in partnership with the Composites Institute of the Society of Plastics Industry, Inc. and in support of the Army’s facility seismic rehabilitation efforts, is investigating the applicability of fiber reinforced polymer (FRP) composite materials systems to strengthen unreinforced masonry (URM) walls. The end product of the research will be the design guidance and construction specifications necessary for the Army to use these materials systems. Much of the Army’s inventory of facilities is constructed of masonry bearing walls. The masonry walls of these facilities are usually either lightly reinforced or unreinforced. This structural system has been shown to perform poorly in past earthquakes and requires upgrading to ensure safety and mission operation during and after an earthquake. This research will develop procedures for the rehabilitation and/or upgrade of masonry walls using typical advanced composite materials systems. New 4-ft by 4-ft double wythe brick wall panels with FRP composite reinforcing applied to one face were constructed and will be tested. The shear performance of different widths and thicknesses of FRP composite applied across brick mortar joints of brick triplets, three brick high prisms with the center brick offset by half an inch, was also tested. Using FRP composites for seismic rehabilitation of URM walls show great potential. Triplet tests showed consistent strengthening of the mortar joints as a function of the width of the FRP composite overlay. With multiple layers of FRP applied, the shear strength of the mortar joints increased sufficiently to cause failure to occur via brick compression failures instead of via shear failure at the mortar joints.