Seismic Retrofit of Reinforced Concrete Columns by Fiber Sheet Wrapping without Removal of Finishing Mortar and Side Wall Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Retrofit of Reinforced Concrete Columns by Fiber Sheet Wrapping without Removal of Finishing Mortar and Side Wall Concrete

Author(s): H. Fukuyama, H. Suzuki, and H. Nakamura

Publication: Symposium Paper

Volume: 188

Issue:

Appears on pages(s): 205-216

Keywords: adhesion; carbon fiber sheet; columns; ductility; finishing mortar; seismic retrofit; shear strength; side wall

DOI: 10.14359/5623

Date: 8/1/1999

Abstract:
In seismic retrofit of existing buildings, there is a great demand that retrofitting work can be done while continuing operations in the building. In order not to disrupt the normal operations in the building, strict limitations on the amount of noise, vibration, dust, and on the use of fire need to be adopted. Since some evaluation methods of retrofitting effects for wrapped RC independent columns with continuous fiber sheets which has an advantage in construction work were proposed, application of this method are dramatically increasing in Japan. However, these evaluation methods can not be applied to the columns with side walls and columns with finishing mortar. When this retrofitting method are applied to these types of columns, finishing is removed and side wall concrete at the boundary portion to the columns is also removed to treat the column with side walls as an independent rectangular column. Then development of the newly effective retrofitting method is necessary to meet the above-mentioned strong demand. This paper reports the test results on the retrofitting effect of RC columns with finishing mortar without removal of finishing and RC columns with side walls without removal of the side wall concrete at the boundary portion. Test results indicates the feasibility of the seismic retrofit of RC columns by fiber sheet wrapping without removal of finishing and side wall concrete.