New Approach for Punching Shear Capacity Prediction of Fiber Reinforced Polymer Reinforced Concrete Flat Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: New Approach for Punching Shear Capacity Prediction of Fiber Reinforced Polymer Reinforced Concrete Flat Slabs

Author(s): A. W. El-Ghandour, K. Pilakoutas, and P. Waldron

Publication: Symposium Paper

Volume: 188

Issue:

Appears on pages(s): 135-144

Keywords: fiber reinforced polymer; punching shear; reinforcement; slabs

DOI: 10.14359/5617

Date: 8/1/1999

Abstract:
In this paper, a new approach predicting the punching shear capacity of FRP reinforced concrete flat slabs without shear reinforcement is introduced in the light of the results of an experimental program conducted at the Centre for Cement and Concrete of the University of Sheffield. The new approach is found to accurately predict the punching shear capacity of the tested slabs. Verification of this new approach is undertaken through comparisons with other test results ensures its validity. Comparisons of the new approach with the ACI 318-95 equation calculating the punching shear capacity of reinforced concrete slabs without shear reinforcement show that the current ACI equation is unconservative in case of FRP reinforcement with low reinforcement ratios. A modification is proposed to the current ACI 318-95 code equation for punching shear in order to accommodate low stiffness FRP reinforcement. Comparisons with test results show that the proposed modification of the ACI code equation leads to good predictions.