Behavior of Embedded Steel Connectors in Concrete Tilt-up Panels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Embedded Steel Connectors in Concrete Tilt-up Panels

Author(s): Kevin Lemieux, Robert Sexsmith, and Gerry Weiler

Publication: Structural Journal

Volume: 95

Issue: 4

Appears on pages(s): 400-411

Keywords: connectors; cyclic tests; embedments; reinforced concrete; static tests; tilt-up panels;

DOI: 10.14359/556

Date: 7/1/1998

Abstract:
The strength and ductility of several tilt-up concrete wall panel connections are investigated analytically and experimentally in a series of monotonic and cyclic tests. For the connectors loaded in tension, experimental results do not support the capacity predictions based on the analysis, due to cone failure in the thin concrete sections. The tension tests showed good agreement in load-deflection behavior between monotonic and cyclic loading, indicating that simple monotonic testing would be adequate for further investigation of the strength and ductility of these connector types. The shear results demonstrated significant differences in load-deflection behavior between monotonic and cyclic loading. Most of the connector types tested did not show sufficient ductility to be used where ductility was a requirement. Further development is needed to produce economical connectors that demonstrate adequate ductility where required