Interrelationships between Reinforcing Bar Physical Properties and Seismic Demands

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Interrelationships between Reinforcing Bar Physical Properties and Seismic Demands

Author(s): J. McDermott

Publication: Symposium Paper

Volume: 184

Issue:

Appears on pages(s): 1-6

Keywords: ductility; modulus of elasticity; reinforcing bar.

DOI: 10.14359/5505

Date: 11/1/1999

Abstract:
Reinforcing bar physical properties are main determinants for reinforcing-bar seismic demands. Consequently, seismic codes set appropriate single upper or lower limits on reinforcing bar yield strength and tensile/yield ratio, but they do not consider the variable-parameter effects of the shape of the reinforcing-bar stress-strain curve on what tensile/yield ratios and ductilities should realistically be required of reinforcing bars in seismic-resistant structures. Therefore, a theoretical study was performed to evaluate the effect of range of allowable steel yield strength, shape of steel stress-strain curve (strain and tangent modulus of elasticity at onset of strain hardening), and beam slenderness (S/d, where S is the clear span length and d is the effective depth to the reinforcing bar centroid, Figure 1) on the minimum values of steel tensile/yield ratio and useful ductility that are necessary to accommodate 2% seismic drift by plastic hinging at the end of beams, Figure 1, of concrete rigid frames reinforced with Grade 60 steel reinforcing bars.