Title: Architectural Precast Concrete Cost Effects

Author(s): Ralph C. Robinson

Publication: Concrete International

Volume: 19

Issue: 8

Appears on pages(s): 25-27

Keywords: architectural concrete; costs; precast concrete;

DOI:

Date: 8/1/1997

Abstract:
This article shows how to reduce costs when using architectural precast concrete. Learn tips to reduce your precast panel costs. Learn the most economical choices regarding shape, corners, weight, panel size, tolerances, and color.