Solidification and Stabilization of Waste Using Portland Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Solidification and Stabilization of Waste Using Portland Cement

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 16

Keywords: waste

DOI:

Date: 10/1/1994

Abstract:
State-of-the-art report on the characteristics of Portland cement and how it can be used effectively to solidify / stabilize various types of wastes. Discusses waste compounds that may interfere with cement hydration reactions. Includes information on several additives that may be used with Portland cement to enhance solidification / stabilization reactions.