Title: C-07: Tilt-Up Construction

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 67

Keywords: tilt-up construction

DOI:

Date: 1/1/1986

Abstract:
Tilt-up construction-fast, efficient, economical. This new compilation offers topics such as: architectural aesthetics of tilt-up panels, connections for tilt-up construction, innovative uses for tilt-up concrete, problems and repairs in tilt-up construction, thermal properties of sandwich panels, and rigging the tilt-up. These are just some of the subjects included in this compilation of articles from Concrete International: Design & Construction.