523.3R-93: Guide for Cellular Concretes Above 50 pcf and for Aggregate Concretes Above 50 pcf with Compressive Strengths Less Than 2500 psi

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 523.3R-93: Guide for Cellular Concretes Above 50 pcf and for Aggregate Concretes Above 50 pcf with Compressive Strengths Less Than 2500 psi

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 16

Keywords: lightweight concrete

DOI:

Date: 1/1/1993

Abstract:

Note: A newer version of this document exists. This document was replaced by 523.3R-14.

Presents information on materials, fabrication, properties, design, and handling of cellular concretes. The usual density range of the concrete considered is 50 pcf to 120 pcf. Concretes in the lower end of this range are generally used for thermal and sound insulation fills for roofs, walls, and floors. The higher densities are used in cast-in-place walls, floors, roofs, and for precast elements.