523.1R-92: Guide for Cast-in-Place Low-Density Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 523.1R-92: Guide for Cast-in-Place Low-Density Concrete

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 8

Keywords: lightweight concrete

DOI:

Date: 3/1/1992

Abstract:

Note: A newer version of this document exists. This document was replaced by 523.1R-06.

This guide provides information on materials, properties, design, and proper handling of cast-in-place concretes having oven-dry unit weights of 50 pcf or less. Such concretes achieve their low weight by the use of low density mineral aggregates or foam and are used to a large extent in roof deck systems.