Title: 506.2-95: Specification for Materials, Proportioning, and Application of Shotcrete

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 8

Keywords: shotcreting

DOI:

Date: 10/1/1995

Abstract:

Note: A newer version of this document exists. This document was replaced by 506.2-13.

This specification contains the construction requirements for the application of shotcrete. Both wet-mix and dry-mix shotcrete are specified, and the minimum standards for testing, materials, and execution are provided.