Behavior and Design of Single Adhesive Anchors under Tensile Load in Uncracked Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior and Design of Single Adhesive Anchors under Tensile Load in Uncracked Concrete

Author(s): Ronald A. Cook, Jacob Kunz, Werner Fuchs, and Robert C. Konz

Publication: Structural Journal

Volume: 95

Issue: 1

Appears on pages(s): 9-26

Keywords: adhesive anchors; adhesives; anchor bolts; anchors; bolts; bonded anchors; chemical anchors; concrete; connections; embedments; fastenings; retrofit;

DOI: 10.14359/522

Date: 1/1/1998

Abstract:
A user-friendly model for the design of single adhesive anchors subjected to tension loading in uncracked concrete is presented. Descriptions of the various types of adhesive anchor systems is included as well as a summary of previously published design models. The development of the user- friendly design model includes a comparison of the model and previously published models to a database including 888 European and American tests. The comparison shows that the simple user-friendly model provides a better fit to the database than more complicated design models previously presented. Although the model is limited to anchors located away from free edges, it provides the basis for development of models which account for the effect of edges, anchor groups, and other design conditions.